Question: 1 / 400

How does contamination affect the performance of tungsten electrodes in welding?

It increases the weld strength

It leads to unstable arc performance

Contamination significantly impacts the performance of tungsten electrodes during welding, and one of the main consequences is that it leads to unstable arc performance. When the tungsten electrode becomes contaminated—often from substances such as oils, grease, or other foreign materials—it can disrupt the arc stability. This instability manifests as erratic arc behavior, which can cause inconsistency in the weld puddle, leading to inadequate heat distribution and increased spatter.

An unstable arc can also result in difficulties in controlling the welding process, which can hamper the operator's ability to produce a uniform and sound weld. Maintaining the integrity of the tungsten electrode by preventing contamination is crucial for achieving a stable arc and ensuring effective weld quality. Therefore, the adverse effects of contamination underscore the importance of proper handling and preparation of tungsten electrodes in Gas Tungsten Arc Welding (GTAW).

Get further explanation with Examzify DeepDiveBeta

It improves the overall quality of the weld

It has no effect on the weld